Very soon after the water and dirt commence to run in the sluice, all the spaces between the riffle-bars are filled .with sand, gravel and dirt; which, however, present many little inequalities of surface sufficient to catch all the particles of gold larger than a pin-head. The largest gold is caught near the head of the sluice; and the farther down the sluioe the finer the gold. In some sluices, where the paydirt contains much coarse gold, the quicksilver is introduced from thirty to sixty yards below the head, so as to catch only the fine particles of metal. CLEANING UP.-The separation of the gold, amalgam and quicksiver from the dirt in the bottom of the sluice is called "cleaning up;" and the period between one "cleaning" up and another is called a "run." A run in a common board sluice usually lasts from six to ten days. Ordinarily the sluice runs only during daylight, but in some claims the work continues night and day. Cleaning up occupies from half a day to a day, and therefore must not be repeated too often, because it consumes too much time. In some sluices the cleaning up does not occur until the rifflebars have been worn out or much bruised by the wear of the stones and gravel. Cleaning up is considered light and pleasant work as compared with sluicing, and is often reserved for Sunday. At the time fixed, the throwing in of dirt ceases, and the water runs until it becomes clear. Five or six sets of riffle-bars, a distance of thirty or thirty-five feet, are taken up at the head of the sluice, and the dirt between the bars is washed down, while the gold and amalgam lodge above the first remaining set of riffle-bars, whence it is taken out with a scoop or large spoon, and put into a pan. Five or six more sets of bars are taken up, and so on down. Sometimes all the riffle-bars are taken up at once, save one set in every 36 feet, and then the work of cleaning up is dispatched much more rapidly. The quicksilver and amalgam taken from the sluice are put into a buckskin or cloth and pressed, so that the liquid metal passes through, and the amalgam is retained. The amalgam is then heated to drive off the mercury. This may be done either in an open pan or in a close retort. In the former the quicksilver is lost; in the latter it is saved. The pan is generally preferred. Often a shovel or plate of iron is used. Three pounds of amalgam, from which the liquid metal has been carefully pressed out, will yield one pound of gold. The gold remaining after the quicksilver has been driven off by heat from the amalgam, is a porous mass, somewhat resembling sponge cake in appearance. RIFFLE-BARS.-The riffle-bars are usually sawn longitudinally with the grain of the wood, but "block riffle-bars" are considered preferable; the latter are cut across the tree, and the grain stands upright in the sluice-box. The block riffle-bars are three times more durable than the longitudinal; and as the latter kind are worn out in a week in sɔme large sluices, there is a considerable saving in using the former. The block riffle-bars are only two or three feet long. In some small sluices the riffle-bars are not placed in the boxes longitudinally, nor in sets; but one bar near the head runs downward at an agle of forty-five degrees to the course of the box, not touching its lower end to the side of the box, but leaving an open space of an inch there. Just below this open space another bar starts from the side of the box and runs downward at right angles to the course of the first bar, and an open space is again left at the end of this bar; and so on down to near the lower end of the sluice, where there are longitudinal riffle-bars in sets as described in the preceding paragraphs. The consequence of using this kind of riffle-bar is, that though much of the water and light dirt runs straight over the bars, the heavier material runs down from side to side in a zigzag course. Near the head of the sluice is a vessel, from which quicksilver falls by drops into the box; and it follows the course of riffle-bars, overtaking the gold which takes the same route. These zigzag riffle-bars are nailed down. In all sluices, men must keep watch to see that the boxes do not choke; that is, that the dirt and stones do not collect in one place, so as to make a dam, and cause the water to run over the sides, and thus waste the gold. There are small sluices, from which all stones as large as a double fist are thrown out. For this purpose the miner uses a sluice-fork, which is like a large manure-fork or garden-fork, but has tines which are blunt and of equal width all the way down; the bluutness being intended to prevent the tines from catching in the wood, and the quality of width to prevent the stones from getting fast in the fork. In some sluices the "block riffle-bars"—that is, bars cut across the grain of the tree-are set transversely in the boxes, and about two inches apart. Another device is, to fill the pores of such riffle-bars with quicksilver. This is done by driving an iron cylinder with a sharp edge into the surface of the bar, then putting mercury into the cylinder, and pressing it into the wood. The quicksilver, thus fastened in the wood, catches particles of gold, which must be scraped off when the time for " cleaning up" comes. DOUBLE SLUICES.-Sluices are sometimes made double -that is, with a longitudinal division through the middle, so that there are two distinct sluice-boxes side by side. Two companies may be working side by side, so that it will be cheaper to build their sluices jointly. In some places the amount of water varies greatly; so that in the winter there is enough to run two sluices, and in the summer only one. And there are companies which wish to continue washing without interruption; so they wash first on one side and then on the other, and clean up without any interruption to the process of washing. Another device for saving gold in sluices is the "undercurrent box." There is a grating of iron bars in the bottom of a box, near the lower end of a sluice; and under this grating is another sluice, with an additional supply of clean. water, and with a lower grade. The grating allows only the fine material to fall through; and the current of water being moderate, many particles of gold, that would otherwise be lost, are saved. Sometimes the matter from the under-current box is led back to the main sluice. ROCK-SLUICES.-Large sluices are frequently paved with stone, which makes a more durable false bottom than wood, and catches fine gold better than riffle-bars. The stone bottoms have another advantage-that it is not so easy for thieves to come and clean up at night, as is often done in riffle-bar sluices. But, on the other hand, cleaning up is more difficult and tedious in a rock-sluice, and so is the putting down of the false bottom after cleaning up. The stones used are cobbles, six or eight inches through at the greatest diameter, and usually flattish. A good workman will pave eight hundred square feet of sluice-box with them in a day; and after the water and dirt have run over them for an hour, they are fastened very tightly by the sand collected between them. In large sluices, wooden riffle-bars are worn away very rapidly—the expense amounting sometimes, in very large and long sluices, to twenty or thirty dollars a day; and in this point there is an important saving by using the stone bottoms. They are used only in large sluices, and they generally have a grade of twelve or fourteen inches to the box of twelve feet. To be Continued. |